DTF chart
| Material | Temperature | Time | Pressure |
|---|---|---|---|
| Cotton and blends | 290–310 °F (145–155 °C) | 8–15 s | Medium–firm |
| Polyester and dry-fit | 285–295 °F (140–145 °C) | 8–12 s | Medium |
| Heavy hoodie | 290–310 °F | 10–15 s | Medium–firm |
| Canvas tote bag | 290–310 °F | 10–15 s | Firm |
| Cap (curved press) | 285–300 °F (140–150 °C) | 10–12 s | Medium |
- Pre-press the garment 3 to 5 seconds to remove moisture.
- After peeling, re-press 5 to 10 seconds with a Teflon sheet or parchment paper.
Sublimation chart
| Product | Temperature | Time | Pressure |
|---|---|---|---|
| Polyester t-shirt | 385–400 °F (195–205 °C) | 40–60 s | Light–medium |
| Ceramic mug (mug press) | 355–400 °F (180–205 °C) | 60–300 s depending on the press | Medium |
| Tumbler (tumbler press) | 365–385 °F (185–195 °C) | 100–120 s | Medium |
| Mouse pad | 375–400 °F (190–205 °C) | 40–45 s | Light–medium |
| Polyester pillow | 385–392 °F (195–200 °C) | 45–60 s | Medium |
| Ceramic tile | 392–400 °F (200–205 °C) | 6–7 min | Medium |
| Aluminum panel | 392–400 °F | 60 s | Medium |
💡 Every press heats differently: check the real temperature with an infrared thermometer and write down the settings that work best.
Temperatures and times are a reference: always check with your supplier and do a test.
Frequently asked questions
Should I peel DTF hot or cold?
It depends on the film: there are cold-peel, hot-peel and both. Follow your supplier's instructions.
Why does the press leave marks?
Too much pressure or a sensitive fabric like polyester. Lower the pressure and use a pressing pillow or Teflon sheet.